Skip to content
BreakingChips

Stainless · ISO M

316 stainless speeds and feeds

Also: SUS316, X5CrNiMo17-12-2, 1.4401, 316S16, S31600

Starting points from the same engines as the calculators, with no tool or setup picked. The first number is where to start; the range is what the manufacturer charts allow. Open a calculator for your tool, machine and cut.

Draft data: researched from manufacturer charts, not yet reviewed by a machinist.

Machining notes

Annealed200 HB

Turning

CutSFMFeed, IPRDepth, in
Finishing625469–781190 m/min0.0060.004–0.0090.16 mm/rev0.0220.004–0.0400.6 mm
Medium525394–656160 m/min0.0120.006–0.0180.31 mm/rev0.0850.012–0.1582.2 mm
Roughing493370–617150 m/min0.0150.009–0.0220.39 mm/rev0.1490.060–0.2373.8 mm

For a CVD carbide insert, general stability, 15 min tool life.

Milling, solid carbide end mill

Speed 180 (100–250) SFM · 55 m/min

Chip load per tooth, before chip thinning
Cutter ØIPTmm/tooth
1/8"0.00030.0001–0.00040.006
1/4"0.00090.0005–0.00130.023
1/2"0.00180.0015–0.00210.046
3/4"0.00290.0028–0.00300.074
1"0.00340.0028–0.00400.086

Drilling, Ø1/2" at 3×D

DrillSFMFeed, IPR
HSS3326–710.00850.0080–0.0090
Cobalt4730–710.00850.0080–0.0090
Solid carbide, through-coolant176100–3000.00530.0050–0.0057

Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.

Tapping

Cut tap
42 (20–80) SFM
Form tap
28 (12–50) SFM

Sources