Non-ferrous · ISO N
6061 aluminum speeds and feeds
Also: EN AW-6061, AlMg1SiCu, A96061
Starting points from the same engines as the calculators, with no tool or setup picked. The first number is where to start; the range is what the manufacturer charts allow. Open a calculator for your tool, machine and cut.
Draft data: researched from manufacturer charts, not yet reviewed by a machinist.
Machining notes
- Sharp, polished uncoated or DLC-coated edges; high speed. Soft tempers are gummy.
T6100 HB
Turning
| Cut | SFM | Feed, IPR | Depth, in |
|---|---|---|---|
| Finishing | 1,9521,171–2,733595 m/min | 0.0070.004–0.0100.18 mm/rev | 0.0220.004–0.0400.6 mm |
| Medium | 1,640984–2,297500 m/min | 0.0140.007–0.0200.34 mm/rev | 0.0850.012–0.1582.2 mm |
| Roughing | 1,542925–2,159470 m/min | 0.0170.010–0.0240.43 mm/rev | 0.1490.060–0.2373.8 mm |
For a UNCOATED carbide insert, general stability, 15 min tool life.
Milling, solid carbide end mill
Speed 800 (500–1,500) SFM · 244 m/min
| Cutter Ø | IPT | mm/tooth |
|---|---|---|
| 1/8" | 0.00110.0010–0.0011 | 0.027 |
| 1/4" | 0.00210.0020–0.0022 | 0.053 |
| 1/2" | 0.00410.0040–0.0042 | 0.104 |
| 3/4" | 0.00730.0060–0.0085 | 0.184 |
| 1" | 0.00810.0070–0.0092 | 0.206 |
Drilling, Ø1/2" at 3×D
| Drill | SFM | Feed, IPR |
|---|---|---|
| HSS | 25089–300 | 0.01050.0070–0.0150 |
| Cobalt | 257177–375 | 0.01050.0070–0.0150 |
| Solid carbide, through-coolant | 651260–1,549 | 0.01350.0080–0.0190 |
Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.
Tapping
- Cut tap
- 55 (30–80) SFM
- Form tap
- 70 (45–90) SFM
O (annealed)60 HB
Turning
| Cut | SFM | Feed, IPR | Depth, in |
|---|---|---|---|
| Finishing | 1,9521,171–2,733595 m/min | 0.0070.004–0.0100.18 mm/rev | 0.0220.004–0.0400.6 mm |
| Medium | 1,640984–2,297500 m/min | 0.0140.007–0.0200.34 mm/rev | 0.0850.012–0.1582.2 mm |
| Roughing | 1,542925–2,159470 m/min | 0.0170.010–0.0240.43 mm/rev | 0.1490.060–0.2373.8 mm |
For a UNCOATED carbide insert, general stability, 15 min tool life.
Milling, solid carbide end mill
Speed 800 (500–1,500) SFM · 244 m/min
| Cutter Ø | IPT | mm/tooth |
|---|---|---|
| 1/8" | 0.00110.0010–0.0011 | 0.027 |
| 1/4" | 0.00210.0020–0.0022 | 0.053 |
| 1/2" | 0.00410.0040–0.0042 | 0.104 |
| 3/4" | 0.00730.0060–0.0085 | 0.184 |
| 1" | 0.00810.0070–0.0092 | 0.206 |
Drilling, Ø1/2" at 3×D
| Drill | SFM | Feed, IPR |
|---|---|---|
| HSS | 25089–300 | 0.01050.0070–0.0150 |
| Cobalt | 257177–375 | 0.01050.0070–0.0150 |
| Solid carbide, through-coolant | 651260–1,549 | 0.01350.0080–0.0190 |
Feeds scale with drill Ø (0.5" here): the drilling calculator sets them for yours.
Tapping
- Cut tap
- 55 (30–80) SFM
- Form tap
- 70 (45–90) SFM
Sources
- Sandvik Coromant — Workpiece materials (MC codes, kc1, mc)
- Mitsubishi Materials USA — Optimum Grades and Chip Breakers for External Turning
- Harvey Tool — General machining guidelines, carbide end mills (SFM and chip load by diameter)
- 6G Tools — Carbide end mill speeds and feeds, general purpose, uncoated (incl. chip load factor)
- Kennametal — HARVI I TE: 5% radial / 2×D axial dynamic milling, 60% / 1.75×D side milling
- Uddeholm — Impax HiHard machining data: slot milling axial depth ≤ 1 × D
- Sandvik Coromant — Formulas and definitions for milling (net power)
- ISCAR — Machining titanium: average chip thickness hm = fz√(ae/d) at light engagement
- Redline Tools — Cobalt & HSS drills (p. 340) and coolant-fed solid carbide drills (p. 328): speeds and feeds
- Viking Drill & Tool — Recommended speeds and feeds for HSS drills
- Hertel (MSC) — High speed steel & cobalt drills: speeds and feeds
- YG-1 — HSS & cobalt drill parameters, and Carbide Dream Drills technical information
- Dormer Pramet (Precision Twist Drill) — R10/R15/R18 general purpose jobber drills: AMG speeds and feeds
- Redline Tools — Cobalt & HSS drills: speeds and feeds (catalog p. 340)
- Sandvik Coromant — Drilling formulas and definitions (net power)
- Haas Tooling — Cobalt jobber drills; carbide drills, general purpose (plain and TSC) and Inox (TSC): feeds and speeds
- OSG — Carbide drills, lists 215/220D/200/233, and HY-PRO CARB coolant-through drills: drilling technical
- Walter Titex — Technical compendium, holemaking 2024: cutting data for solid carbide drills
- Ingersoll — WinTwist exchangeable-head drills: operating guidelines (NEW-393-2, pp. 9–10)
- Tru-Edge — Solid carbide drills: feeds and speeds
- YG-1 — Carbide Dream Drills: technical information (speeds, feeds, depth factors)
- OSG — HY-PRO and HY-PRO NRT taps: recommended tapping conditions
- Haas Tooling — Taps and roll taps: speeds and feeds by ISO material group