Skip to content
BreakingChips

ISO metric · fine

M36 × 1.5 tap drill size

For general work, OSG suggests 65–70% of full thread. Harder materials and deep holes want less; the calculator sets it from your material.

Cut tap

34.5 mm

1.3583" · 77% thread

Form tap

35.5 mm

1.3976" · 49% thread

Or 1-25/64 (1.3906") for 66%

Open M36 × 1.5 in the calculator

Pick your material for its % of thread, tapping RPM and the rigid-tap code.

Thread dimensions

Major Ø
36.000 mm (1.4173")
Pitch
1.5 mm
Pitch Ø (basic)
35.026 mm (1.3790")
Minor Ø (internal, basic)
34.376 mm (1.3534")
Thread depth (internal)
0.812 mm (0.0320")

Basic sizes of the 60° form. Tolerance classes (6H) set the limits around them.

Cut tap drills

For a cutting (fluted or spiral) tap. Every standard drill from 50% to 85% thread; suggested rows are in the 65–70% band.

Cut tap drills for M36 × 1.5
DrillØ inØ mmThread
34.5 mm1.358334.5077%
1-23/641.359434.5376%
1-3/81.375034.9355%
35 mm1.378035.0051%

Form tap drills

A form (roll) tap displaces metal instead of cutting it, so it needs a bigger hole. Every standard drill from 50% to 85% thread; suggested rows are in the 65–70% band.

Form tap drills for M36 × 1.5
DrillØ inØ mmThread
1-25/64suggested1.390635.3266%

3-wire measurement

Best wire size
0.866 mm (0.0341")
Over wires, at basic pitch Ø
36.325 mm (1.4301")

For the external thread (the screw). The best wire touches the flanks at the pitch diameter.

Sources